>Stainless Steel

NC-308LSi
For Austenitic stainless steel welding electrode
- AWS
 - A5.4 E308L-17
 
- KS
 - D 7014 E308L-16
 
- JIS
 - Z 3221 ES308L-17
 
- EN
 - ISO 3581-A E 19 9 L R 1 2
ISO 3581-B ES308L-17 
| Applications | 18% Cr-8% Ni stainless steel such as AISI(SUS) 304L | 
|---|---|
| Characteristics | 1.Covering is lime titania type for welding of AISI(SUS) 304L and for the same purpose as NC-308. 2. Covering type is 17 and weldability is very good, especially it has concave bead in horizontal fillet welding. 3. As its weld metal a extra-low carbon austenitic structure which contains suitable ferrite, crack resistibility is good and intergranular corrosion resistibility is superior to that of NC-308. 4. AC or DC (+) polarity is used, especially weldability is better in DC (+).  | 
				
| Notes on usage | 1. When the electrodes have absorbed moisture, dry them at 250-300℃ for 60-90 minutes before use. 2. Keep the arc as short as possible. 3. Remove dirt such as oil and dust from the groove before welding.  | 
				
| Shielding Gas | - | 



		