>Mild & High Tensile Steel
CSF-70T5
For mild steel and 490N/mm2 class high tensile strength steel
- AWS
- A5.20 E70T-5M-J
- KS
- D 7104 YFW-A502B
- JIS
- Z 3313 T49J4T5-0MA-U
- EN
- ISO 17632-A T42 4 B M 3 H5
ISO 17632-B T49 4 T5-0 M A-UH5
Applications | Butt, fillet welding of 490N/mm2 high tensile strength steels of structure such as ships, iron structure, buildings etc. |
---|---|
Characteristics | 1) CSF-70T5 is Basic Slag type. (2) Low temperature impact value and crack-resistance is superior by product that is alternated in arc electrode's 7018 precincts. |
Notes on usage | (1) The optimum flow rate of Mix gas for shielding is 20~25ℓ/min. (2) Protect the weld with a screen to prevent blowholes caused by wind where the wind velocity is 2m/sec and more. (3) Keep the distance between tip & base metal at 15~25mm. |
Shielding Gas | 80%Ar-20%CO2 |