>Nickel and Nickel alloy
CSI-625
CSI-625 is designed to match inconel 625, incoloy 825, incoloy 25-6Mo and other Mo containingstainless steel. Suitable in pressure vessel fabrication for -196℃ to 550℃, otherwiseup to the scaling resistance temperature of 1200℃.The weld metal has high strength at room and elevated temperatures and has exceptionalcorrosion resistance, including resistance to pitting, crevice corrosion and polythionic acidstress-corrosion cracking. CSI-625 is useful for many dissimilar joints involving inconel alloys,incoloy alloys, stainless steels, low-alloy steel, and carbon steel.
- AWS
- A5.11 ENiCrMo-3
- KS
- -
- JIS
- Z 3224 E Ni 6182
- EN
- ISO 14172 E Ni 6625 (NiCr22Mo9Nb)
Applications | For high temperature and creep resisting steel, heat resisting and dissimilar joint. |
---|---|
Characteristics | CSI-625 is designed to match inconel 625, incoloy 825, incoloy 25-6Mo and other Mo containing stainless steel. Suitable in pressure vessel fabrication for -196℃ to 550℃, otherwise up to the scaling resistance temperature of 1200℃. The weld metal has high strength at room and elevated temperatures and has exceptional corrosion resistance, including resistance to pitting, crevice corrosion and polythionic acid stress-corrosion cracking. CSI-625 is useful for many dissimilar joints involving inconel alloys, incoloy alloys, stainless steels, low-alloy steel, and carbon steel. |
Notes on usage | (1) Use recommended current range. if not it will be much spatters and undercut. (2) Keep the arc as short as possible. (3) Weaving width should be within two and a half times electrode's diameter. (4) When the electrodes have absorbed moisture, dry them at 250~280℃ for 30~60 minutes before use. |
Shielding Gas | - |